Polymer Property : Compressive Modulus = 16700 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 115 - 115 GPa

@Temperature 70.0 - 70.0 °C
16700 - 16700 ksi

@Temperature 158 - 158 °F
Average value: 115 GPa Grade Count:1
Overview of materials for Epoxy Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive". Each property range of values reported is minimum and maximum values of appropriate Mat..