Mechanical Properties Metric English Comments
Compressive Modulus 2.18 GPa
316 ksi
ASTM D695
Quadrant EPP PPO Polyphenylene oxide, unfilled, extruded (ASTM Product Data Sheet)
Data provided by Quadrant Engineering Plastic Products.