Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 2.21 GPa | 320 ksi | ASTM D695 |
Quadrant EPP Nylatron® MD PA6, Metal-detectable Nylon (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic Products Broadest size range availability Good mechanical and electrical properties Ideal balance of strength and toughness Cast as finished parts and n.. |
|||
Compressive Modulus | 2.21 GPa | 321 ksi | |
Abatron AboCast 8103-16 One Part Epoxy One component system. Less viscous than 8103-11. Information provided by Abatron, Inc.Processing: Shelf life 6-8 months at 25°C (77°F). Heat cured; Pot life 360 min. at 100°C (212°C). Peak e.. |