Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 2.85 GPa | 413 ksi | DIN EN ISO 604 |
Wolf Kunststoff ZEDEX® ZX-324V11T A3L PEEK Polymer, Reinforced Main Charactistics: Stress resistant; High impact strength at 196 ° C Applications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInformation provided by Zedex |
|||
Compressive Modulus | 2.85 GPa | 413 ksi | ASTM D695 |
DuPont Teijin Films Mylar® A Polyester Film, 1000 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |