Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 2.942 GPa | 426.7 ksi | ASTM D695 |
Daelim H&L Plavis-G15 ISO 15% Graphite Filled Aromatic Polyimide Bearing Isostatically Molded. Plavis-G-15: Graphite 15 wt% filled, Self lubricating grade for wear and friction applications.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded .. |