Polymer Property : Compressive Modulus = 209.7 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 1.446 GPa

@Temperature 23.0 °C
209.7 ksi

@Temperature 73.4 °F
EN ISO 604
Ensinger TECASINT™ 2032 Polyimide, Black, 40% Graphite (PI)
TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications...