Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 21.4 GPa @Temperature 23.9 °C |
3100 ksi @Temperature 75.0 °F |
Dry; 325°F Autoclave; ASTM D695 |
Park Electrochemical Nelcote® F-554 Phenolic Prepreg, Commercial Silica Fabric Reinforced Nelcote® F-554 is a high purity silica filled phenolic resin coated on Commercial or Aerospace grade silica fabric. F-554 is used in the manufacture of intermediate temperature ablative rocket nozz.. |
|||
Compressive Modulus | 21.4 GPa @Temperature 23.9 °C |
3100 ksi @Temperature 75.0 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® F-562 Phenolic Prepreg, 8HS Silica Reinforced Nelcote® F-562 is an elastomer modified phenolic resin used in the manufacture of intermediate temperature ablative rocket nozzles, heat shields and combustion chambers in highly oxidative environm.. |