Compressive Modulus
1.50
GPa
217
ksi
Abatron AboCast 50-6/AboCure 50-17 Epoxy
Data provided by the manufacturer, Abatron, Inc. Very low-viscosity; Medium Amber color. Shelf life is 12+ months.