Polymer Property : Compressive Modulus = 26.8 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 0.185 GPa
26.8 ksi
Loading, In the Through Plane Direction
Cymat A35620SC 020SS Stabilized Aluminum Foam
Description: Cymat A35620SC 020SS stabilized aluminum foam (SAF) is a closed cell aluminum foam formed from A356 aluminum alloy with a density of 0.2 g/cm3. The mechanical properties of SAF make it ..