Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 3.10 GPa | 450 ksi | ASTM D695 |
Quadrant EPP Acetron® POM-H Homopolymer Acetal, Unfilled, Extruded (ASTM Product Data Sheet) |
|||
Compressive Modulus | 3.10 GPa | 450 ksi | ASTM D695 |
Saint-Gobain Meldin® 5055 Thermoplastic Bearing Material General Notes on Meldin 3000/5000 Series Bearing Products:Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water.Specific Notes on Meldin.. |
|||
Compressive Modulus | 3.10 GPa | 450 ksi | ASTM D695 |
Saint-Gobain Meldin® 7021 CM Compression Molded Graphite Filled Polyimide Melidin® 7021 CM is a self-lubricating compression molded polyimide that contains 15% graphite filler. Melidin® 7021 has a low coefficient of friction and high heat resistance, and is best fo.. |
|||
Compressive Modulus | 3.10 GPa | 450 ksi | ASTM D695 |
Ensinger Tecapeek® XP-119 Compression Molded PEEK Compound, 10% Carbon Fiber Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Compressive Modulus | 3.10 GPa | 450 ksi | ASTM D695 |
Quantum Acetal-Homopolymer Information provided by Quantum Advanced Engineering Plastics |
|||
Compressive Modulus | 3.10 GPa | 450 ksi | TM R050-38 |
Resinlab® EP1306 Acrylic / Epoxy Hybrid Adhesive EP1306 is a two part acrylic / epoxy hybrid adhesive utilizing a 50% weight loading of aluminum powder into both components. It cures quickly at room temperature to a tough, rigid polymer. It has go.. |