Mechanical Properties Metric English Comments
Compressive Modulus 210 GPa
30500 ksi
Specialty Materials 5505 Boron Epoxy Prepreg Tape
Specialty Materials' 5505 is a highly advanced prepreg tape, combining Specialty Materials' 4.0 or 5.6 mil boron filament with a tough, rigid, epoxy resin. Exhibiting exceptional performance at temp..
Compressive Modulus 210 GPa
30500 ksi
Specialty Materials 5521 Boron Epoxy Prepreg Tape
Specialty Materials' 5521 is a highly advanced prepreg tape, combining Specialty Materials' 4.0 or 5.6 mil boron filament with a tough, rigid, epoxy resin. Performing at temperatures up to 350°F,..