Polymer Property : Compressive Modulus = 334 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 2.30 GPa
334 ksi
ASTM D695
Saint-Gobain Meldin® 7021 Isostatically Molded Graphite Filled Polyimide
Melidin® 7021 is a self-lubricating thermosetting polyimide that contains 15% graphite filler. Melidin® 7021 has a low coefficient of friction and high heat resistance, and is best for high t..
Compressive Modulus 2.30 GPa
334 ksi
ASTM D695
Saint-Gobain Meldin® 7211 Isostatically Molded Graphite and PTFE Filled Polyimide
Finished parts and basic shapes made from 10% by weight PTFE and 15% by weight graphite filled polyimide material for applications requiring a very low coefficient of friction and self-lubricating p..
Compressive Modulus 2.30 GPa
334 ksi
Abatron AboCast 8103-11 One Part Epoxy
One component system. Information provided by Abatron, Inc.Processing: Shelf life 6-8 months at 25°C (77°F). Heat cured; Pot life 190 min. at 100°C (212°C). Peak exotherm 170°C (340°F). At..