Compressive Modulus 2.403 GPa
348.5 ksi
ASTM D695
Daelim H&L Plavis-N DF Unfilled Aromatic Polyimide Bearing
Direct Formed. Plavis-N: Best physical properties, maximum electrical and thermal insulation, low out-gassing, superior radiation resistance.General Plavis information for all grades:PLAVIS polyimi..