Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 26.9 GPa @Temperature 21.1 °C |
3900 ksi @Temperature 70.0 °F |
Dry; ASTM D695 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, Spectra® 951 - PT Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |