Polymer Property : Compressive Modulus = 4.317 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 4.317 GPa
626.2 ksi
ASTM D695
Ensinger Tecapeek® XP-98ST Compression Molded PEEK ST, 30% Carbon Fiber
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..