Mechanical Properties Metric English Comments
Compressive Modulus 53.0 GPa

@Temperature 75.0 °C
7690 ksi

@Temperature 167 °F
Wet; DIN65380
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 45% 46280 Fiber
Information provided by HexCel
Compressive Modulus 53.0 GPa

@Temperature 75.0 °C
7690 ksi

@Temperature 167 °F
Wet; DIN65380
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, TVR380/26% Fiber
Information provided by HexCel