Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 57.2 GPa @Temperature 21.1 °C |
8300 ksi @Temperature 70.0 °F |
Dry; Vacuum/Oven Cured; SACMA 1-94 |
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T700 12K BW Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Compressive Modulus | 57.2 GPa @Temperature 24.0 °C |
8300 ksi @Temperature 75.2 °F |
|
Hexcel® HexPly® F155 Epoxy Resin, W3T282 Carbon Fabric Hexcel designation: W3T282-42"-F155; Fiber: T300 Toho®Information provided by HexCel |