Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Modulus = 580.9 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 4.005 GPa
580.9 ksi
perpendicular to plane; ASTM C365
3A Composites Core Materials BALTEK® SB.100 Structural End-Grain Balsa
BALTEK SB is a core material produced from certified kiln-dried balsa wood in the ‘end-grain’ confiation. It has extremely high strength and stiffness to weight ratios, and achieves an excellent b..
Copyright © lookpolymers.com All Rights Reserved