Polymer Property : Compressive Modulus = 63.8 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 0.440 GPa
63.8 ksi
ASTM D695
3M Dyneon™ CC604 PTFE, 20% Fiberglass Filled  (discontinued **)
Product Form: White, pelletized free-flowing powder. Applications include bearings, valve seats, seals.Data provided by Dyneon.
Compressive Modulus 0.440 GPa
63.8 ksi
ASTM D695
Manifattura Cattaneo RULON® LR Polytetrafluoroethylene
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.