Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 66.9 GPa @Temperature 23.9 °C |
9700 ksi @Temperature 75.0 °F |
Dry; Oven Cure 275°F, 90 min; ASTM D695 |
Park Electrochemical Nelcote® E-763 Epoxy Prepreg, 3K 2x2 Twill Carbon Reinforced Nelcote® E-763 is a modified epoxy system with a nominal 250°F cure temperature. E-763 provides a transparent resin surface on the finished part which gives finished part surfaces a cosmetic attra.. |
|||
Compressive Modulus | 66.9 GPa @Temperature 24.0 °C |
9700 ksi @Temperature 75.2 °F |
Dry |
Hexcel® HexPly® F522 Epoxy Resin, F3C584 Carbon Fabric Hexcel designation: F3C584-42"-F522; Fiber: Toho® G30/500-3KInformation provided by HexCel |