Polymer Property : Compressive Modulus = 7.982 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 7.982 GPa
1158 ksi
perpendicular to plane; ASTM C365
3A Composites Core Materials BALTEK® SB.150 Structural End-Grain Balsa
BALTEK SB is a core material produced from certified kiln-dried balsa wood in the ‘end-grain’ confiation. It has extremely high strength and stiffness to weight ratios, and achieves an excellent b..