Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 4.31 - 6.47 GPa | 625 - 938 ksi | Average value: 5.75 GPa Grade Count:3 |
Overview of materials for Polyetherimide (PEI), 30% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 30% Glass Fiber". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Compressive Modulus | 0.0460 - 6.47 GPa | 6.67 - 938 ksi | Average value: 3.28 GPa Grade Count:21 |
Overview of materials for Polyetherimide (PEI) This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat.. |