Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.0333 GPa @Strain 34.93 %, Temperature 100 °C |
4.82 ksi @Strain 34.93 %, Temperature 212 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC4601 NC010 Nylon
(Unverified Data**) Plasticized Toughened Renewably Sourced Polyamide Developed for Extrusion Zytel RS LC4601 NC010 is a flexible toughened and plasticized polyamide resin intended for extrusion applications.Informatio.. |