Mechanical Properties Metric English Comments
Secant Modulus 0.0786 GPa

@Strain 29.03 %,
Temperature 40.0 °C
11.4 ksi

@Strain 29.03 %,
Temperature 104 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® LC6200 BK385 Nylon 612  (Unverified Data**)
Toughened Polyamide 612 Developed for ExtrusionInformation provided by DuPont Performance Polymers