Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.150 GPa @Strain 6.34 %, Temperature 40.0 °C |
21.7 ksi @Strain 6.34 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC4601 NC010 Nylon
(Unverified Data**) Plasticized Toughened Renewably Sourced Polyamide Developed for Extrusion Zytel RS LC4601 NC010 is a flexible toughened and plasticized polyamide resin intended for extrusion applications.Informatio.. |
|||
Secant Modulus | 0.150 GPa @Strain 14.39 %, Temperature 100 °C |
21.7 ksi @Strain 14.39 %, Temperature 212 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 444AHS BK152 Nylon 66
(Unverified Data**) Toughened Heat Stabilized Polyamide 66 Zytel 444AHS is a toughened heat stabilized black polyamide 66 resin for injection molding. It is a high flow processing friendly material.Information provided.. |