Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.233 GPa @Strain 16.51 %, Temperature 100 °C |
33.8 ksi @Strain 16.51 %, Temperature 212 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 132F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 132F NC010 is a nucleated lubricated polyamide 66 for injection molding. It was developed for fast production cycles and high productivity applications.Info.. |
|||
Secant Modulus | 0.233 GPa @Strain 14.0 %, Temperature 80.0 °C |
33.8 ksi @Strain 14.0 %, Temperature 176 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 12T NC010 Nylon 66
(Unverified Data**) 36% Mineral Reinforced Toughened Polyamide 66 Minlon 12T NC010 is a 36% mineral reinforced toughened heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performan.. |