Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.582 GPa @Strain 7.00 %, Temperature 23.0 °C |
84.4 ksi @Strain 7.00 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® ST830FRUV NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Flame Retardant UV Stabilized Polybutylene Terephthalate Crastin ST830FRUV NC010 is an unreinforced Super Tough flame retardant polybutylene terephthalate resin for injection molding. I.. |