Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 0.792 GPa @Strain 3.70 %, Temperature 80.0 °C |
115 ksi @Strain 3.70 %, Temperature 176 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 11C40 NC010 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Polyamide 66 Minlon 11C40 NC010 is a 40% mineral reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |