Polymer Property : Secant Modulus = 1.05 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 1.05 GPa

@Strain 2.10 %,
Temperature 40.0 °C
152 ksi

@Strain 2.10 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® S600F20 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S600F20 NC010 is an unreinforced lubricated medium viscosity polybutylene terephthalate resin for injection molding.Information provi..
Secant Modulus 1.05 GPa

@Strain 2.10 %,
Temperature 40.0 °C
152 ksi

@Strain 2.10 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® S600F20UV WT660 Polybutylene Terephthalate (PBT)
Unreinforced UV Stabilized Polybutylene Terephthalate Crastin S600F20 NC010 is an unreinforced lubricated medium viscosity polybutylene terephthalate resin for injection molding.Information provided..
Secant Modulus 1.05 GPa

@Strain 1.20 %,
Temperature 80.0 °C
152 ksi

@Strain 1.20 %,
Temperature 176 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 127UV NC010 Acetal (POM)  (Unverified Data**)
UV Stabilized High Viscosity Acetal HomopolymerDelrin 127UV is a high viscosity acetal homopolymer with UV stabilizers developed for automotive interior applications. It has improvements in UV aging..
Secant Modulus 1.05 GPa

@Strain 3.50 %,
Temperature 100 °C
152 ksi

@Strain 3.50 %,
Temperature 212 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK641FR NC010 Polybutylene Terephthalate (PBT)
10% Glass Reinforced Flame Retardant Polybutylene Terephthalate Information provided by DuPont Performance Polymers
Secant Modulus 1.05 GPa

@Strain 2.40 %,
Temperature 40.0 °C
153 ksi

@Strain 2.40 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® ST830FRUV NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced Flame Retardant UV Stabilized Polybutylene Terephthalate Crastin ST830FRUV NC010 is an unreinforced Super Tough flame retardant polybutylene terephthalate resin for injection molding. I..