Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 1.36 GPa @Strain 2.68 %, Temperature 0.000 °C |
197 ksi @Strain 2.68 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® BM6450XD BK560 Polybutylene Terephthalate (PBT)
(Unverified Data**)& Unreinforced Polybutylene Terephthalate Developed for Blow MoldingCrastin BM6450XD BK560 is an unreinforced supertough polybutylene terephthalate resin with very high viscosity for extrusion and blo.. |
|||
Secant Modulus | 1.36 GPa @Strain 0.900 %, Temperature 80.0 °C |
197 ksi @Strain 0.900 %, Temperature 176 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 900P BK602 Acetal (POM)
(Unverified Data**) Low Viscosity Acetal Homopolymer with Improved ProcessingDelrin 900P BK602 is a low viscosity black acetal homopolymer resin for multicavity and thin wall molding. It offers an improved processing t.. |
|||
Secant Modulus | 1.36 GPa @Strain 1.0187 %, Temperature 80.0 °C |
198 ksi @Strain 1.0187 %, Temperature 176 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG500P NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG500P is a medium viscosity acetal homopolymer with improved thermal stability. It has been developed for consider.. |
|||
Secant Modulus | 1.36 GPa @Strain 6.00 %, Temperature 0.000 °C |
197 ksi @Strain 6.00 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500PE NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE NC010 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi.. |