Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 1.71 GPa @Strain 4.13 %, Temperature 200 °C |
248 ksi @Strain 4.13 %, Temperature 392 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 92G45DH2 BK083 Polyphthalamide (PPA) 35% Glass Reinforced PPA High Performance Polyamide with DuPont Zytel HTN92G45DH2 BK083 is a 45% glass reinforced high performance polyamide resin using DuPont SHIELD Technology with high flow and e.. |
|||
Secant Modulus | 1.71 GPa @Strain 3.00 %, Temperature 100 °C |
248 ksi @Strain 3.00 %, Temperature 212 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® IG38C1 BK434 Nylon 66
(Unverified Data**) 38% Mineral/Glass Reinforced Polyamide 66 Minlon IG38C1 BK434 is a 38% mineral/glass reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont Performa.. |