Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 7.20 GPa @Strain 1.05 %, Temperature 40.0 °C |
1040 ksi @Strain 1.05 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9030FR NC010 PBT+ASA
(Unverified Data**) 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030FR NC010 is a 30% glass fiber reinforced flame retardant polybutylene terephthal.. |
|||
Secant Modulus | 7.20 GPa @Strain 0.300 %, Temperature 23.0 °C |
1040 ksi @Strain 0.300 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK603 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Crastin SK603 NC010 is a 20% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Secant Modulus | 7.20 GPa @Strain 1.50 %, Temperature -20.0 °C |
1040 ksi @Strain 1.50 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK643FR NC010 Polybutylene Terephthalate (PBT) 20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK643FR is a flame retardant 20% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.8.. |
|||
Secant Modulus | 7.16 GPa @Strain 1.11 %, Temperature 0.000 °C |
1040 ksi @Strain 1.11 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 935SUV BK593 Polyethylene Terephthalate (PET)
(Unverified Data**) 35% Glass Reinforced UV Stabilized Polyethylene Terephthalate Rynite 935SUV BK593 is a 35% glass fiber /mineral reinforced UV stabilized modified polyethylene terephthalate resin with low warpage de.. |
|||
Secant Modulus | 7.14 GPa @Strain 1.27 %, Temperature 40.0 °C |
1040 ksi @Strain 1.27 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FR52G30NH NC010 Polyphthalamide (PPA)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G30NH NC010 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin. It.. |
|||
Secant Modulus | 7.16 GPa @Strain 1.61 %, Temperature 23.0 °C |
1040 ksi @Strain 1.61 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FR52G30NH NC010 Polyphthalamide (PPA)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G30NH NC010 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin. It.. |