Mechanical Properties Metric English Comments
Secant Modulus 8.93 GPa

@Strain 1.30 %,
Temperature -40.0 °C
1300 ksi

@Strain 1.30 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® 935SUV BK593 Polyethylene Terephthalate (PET)  (Unverified Data**)
35% Glass Reinforced UV Stabilized Polyethylene Terephthalate Rynite 935SUV BK593 is a 35% glass fiber /mineral reinforced UV stabilized modified polyethylene terephthalate resin with low warpage de..
Secant Modulus 8.95 GPa

@Strain 0.860 %,
Temperature -20.0 °C
1300 ksi

@Strain 0.860 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® GW520CS NC010 Polyethylene Terephthalate (PET)
20% Glass Reinforced Flame Retardant Polyethylene Terephthalate with Improved Glow Wire Performance Rynite GW520CS NC010 is a 20% glass fiber reinforced flame retardant color stabilized modified pol..
Secant Modulus 8.97 GPa

@Strain 1.36 %,
Temperature -20.0 °C
1300 ksi

@Strain 1.36 %,
Temperature -4.00 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 73G30T NC010 Nylon 6  (Unverified Data**)
30% Glass Reinforced Toughened Polyamide 6 Zytel 73G30T NC010 is a 30% glass fiber reinforced toughened polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Secant Modulus 8.97 GPa

@Strain 0.310 %,
Temperature -20.0 °C
1300 ksi

@Strain 0.310 %,
Temperature -4.00 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G25HSL NC010 Nylon 66  (Unverified Data**)
25% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G25HSL NC010 is a 25% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perform..