Mechanical Properties Metric English Comments
Secant Modulus 10.0 GPa

@Strain 0.210 %,
Temperature 40.0 °C
1450 ksi

@Strain 0.210 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK608 BK509 Polybutylene Terephthalate (PBT)  (Unverified Data**)
45% Glass Reinforced Polybutylene Terephthalate Crastin SK608 BK509 is a 45% glass fiber reinforced lubricated black polybutylene terephthalate resin for injection molding.Information provided by Du..
Secant Modulus 9.98 GPa

@Strain 0.700 %,
Temperature 23.0 °C
1450 ksi

@Strain 0.700 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT)
30% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on pol..
Secant Modulus 9.98 GPa

@Strain 0.700 %,
Temperature 23.0 °C
1450 ksi

@Strain 0.700 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Sorona® 3030G NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&
30% Glass Reinforced Polytrimethylene Terephthalate Sorona 3030G NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with goo..
Secant Modulus 9.99 GPa

@Strain 0.453926 %,
Temperature 0.000 °C
1450 ksi

@Strain 0.453926 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK615SF NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
30% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK615SF is a 30% glass fiber reinforced low viscosity polybutylene terephthalate for injecti..
Secant Modulus 9.98 GPa

@Strain 1.57 %,
Temperature -40.0 °C
1450 ksi

@Strain 1.57 %,
Temperature -40.0 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® EFE7374 BK416 Nylon 6  (Unverified Data**)