Mechanical Properties Metric English Comments
Secant Modulus 10.358 GPa

@Strain 0.500 %,
Temperature 23.0 °C
1502.3 ksi

@Strain 0.500 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 74G33W BK196 Nylon 66  (Unverified Data**)
33% Glass Reinforced UV Stabilized Polyamide 66 + Polyamide 6 Zytel 74G33W BK196 is a high gloss automotive weatherable black 33% glass reinforced nylon 66 and nylon 6 comelt resin.Information provi..