Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 1.13 GPa @Strain 1.27 %, Temperature 40.0 °C |
164 ksi @Strain 1.27 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® 6129 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection MoldingInformation provided by DuPont Performance Polymers |
|||
Secant Modulus | 1.13 GPa @Strain 1.27 %, Temperature 40.0 °C |
164 ksi @Strain 1.27 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® 6130 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin 6130 NC010 is an unreinforced medium high viscosity polybutylene terephthalate resin for .. |