Polymer Property : Secant Modulus = 168 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 1.16 GPa

@Strain 1.90 %,
Temperature 40.0 °C
168 ksi

@Strain 1.90 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 100T NC010 Acetal (POM)  (Unverified Data**)
Toughened High Viscosity Acetal Homopolymer Delrin 100T NC010 is a toughened high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers
Secant Modulus 1.16 GPa

@Strain 2.50 %,
Temperature 23.0 °C
168 ksi

@Strain 2.50 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 100T NC010 Acetal (POM)  (Unverified Data**)
Toughened High Viscosity Acetal Homopolymer Delrin 100T NC010 is a toughened high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers
Secant Modulus 1.16 GPa

@Strain 5.56 %,
Temperature 23.0 °C
168 ksi

@Strain 5.56 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 300CP NC010 Acetal (POM)  (Unverified Data**)
Medium-high Viscosity Acetal Homopolymer with Improved ProcessingDelrin 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of proc..
Secant Modulus 1.16 GPa

@Strain 6.89 %,
Temperature -20.0 °C
168 ksi

@Strain 6.89 %,
Temperature -4.00 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 444AHS BK152 Nylon 66  (Unverified Data**)
Toughened Heat Stabilized Polyamide 66 Zytel 444AHS is a toughened heat stabilized black polyamide 66 resin for injection molding. It is a high flow processing friendly material.Information provided..
Secant Modulus 1.16 GPa

@Strain 0.180 %,
Temperature 0.000 °C
168 ksi

@Strain 0.180 %,
Temperature 32.0 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS LC1600 NC010 Nylon 1010
Plasticized Toughened UV Stabilized Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1600 NC010 is a renewable sourced Polyamide 1010 containing a minimum of 60% renewably sourced..