Polymer Property : Secant Modulus = 174 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 1.20 GPa

@Strain 7.00 %,
Temperature 100 °C
174 ksi

@Strain 7.00 %,
Temperature 212 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 74G33W BK196 Nylon 66  (Unverified Data**)
33% Glass Reinforced UV Stabilized Polyamide 66 + Polyamide 6 Zytel 74G33W BK196 is a high gloss automotive weatherable black 33% glass reinforced nylon 66 and nylon 6 comelt resin.Information provi..
Secant Modulus 1.20 GPa

@Strain 3.50 %,
Temperature 80.0 °C
174 ksi

@Strain 3.50 %,
Temperature 176 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK641FR NC010 Polybutylene Terephthalate (PBT)
10% Glass Reinforced Flame Retardant Polybutylene Terephthalate Information provided by DuPont Performance Polymers