Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 13.4 GPa @Strain 1.05 %, Temperature 23.0 °C |
1950 ksi @Strain 1.05 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 92G45DH2 BK083 Polyphthalamide (PPA) 35% Glass Reinforced PPA High Performance Polyamide with DuPont Zytel HTN92G45DH2 BK083 is a 45% glass reinforced high performance polyamide resin using DuPont SHIELD Technology with high flow and e.. |
|||
Secant Modulus | 13.4 GPa @Strain 0.240 %, Temperature 0.000 °C |
1950 ksi @Strain 0.240 %, Temperature 32.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 92G45DH2 BK083 Polyphthalamide (PPA) 35% Glass Reinforced PPA High Performance Polyamide with DuPont Zytel HTN92G45DH2 BK083 is a 45% glass reinforced high performance polyamide resin using DuPont SHIELD Technology with high flow and e.. |