Secant Modulus 2.17 GPa

@Strain 2.40 %,
Temperature 0.000 °C
314 ksi

@Strain 2.40 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 100P NC010 Acetal (POM)  (Unverified Data**)
High Viscosity Acetal Homopolymer with Improved Processing Delrin 100P is a high viscosity acetal homopolymer for use in easy to fill molds. It has improved processing thermal stability good mechani..
Secant Modulus 2.17 GPa

@Strain 1.71 %,
Temperature 40.0 °C
314 ksi

@Strain 1.71 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 311DP NC010 Acetal (POM)  (Unverified Data**)
Nucleated Medium-high Viscosity Acetal Homopolymer Delrin 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization and balance of part performance and ease of processing. It..
Secant Modulus 2.17 GPa

@Strain 3.70 %,
Temperature -40.0 °C
315 ksi

@Strain 3.70 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500P BK602 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer with Improved ProcessingDelrin 500P BK602 is a general purpose medium viscosity black acetal homopolymer resin for injection molding. Delrin 500P has improved pro..
Secant Modulus 2.17 GPa

@Strain 2.40 %,
Temperature 0.000 °C
314 ksi

@Strain 2.40 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG100P NC010 Acetal (POM)  (Unverified Data**)
High Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG100P is a high viscosity acetal homopolymer with improved thermal stability for use in easy to fill molds. It has b..
Secant Modulus 2.17 GPa

@Strain 1.71 %,
Temperature 40.0 °C
314 ksi

@Strain 1.71 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG311DP NC010 Acetal (POM)  (Unverified Data**)
Nucleated Medium-high Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG311DP is a medium-high viscosity acetal homopolymer with improved thermal stability and modificati..
Secant Modulus 2.17 GPa

@Strain 1.92 %,
Temperature 40.0 °C
314 ksi

@Strain 1.92 %,
Temperature 104 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66  (Unverified Data**)
Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe..