Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 2.26 GPa @Strain 1.70 %, Temperature 0.000 °C |
328 ksi @Strain 1.70 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 520MP NC010 Acetal (POM)
(Unverified Data**) 20% Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 520MP is a medium viscosity acetal homopolymer containing 20% Teflon PTFE Micropowder. It is designe.. |
|||
Secant Modulus | 2.26 GPa @Strain 2.82 %, Temperature 200 °C |
327 ksi @Strain 2.82 %, Temperature 392 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 92G45DH2 BK083 Polyphthalamide (PPA) 35% Glass Reinforced PPA High Performance Polyamide with DuPont Zytel HTN92G45DH2 BK083 is a 45% glass reinforced high performance polyamide resin using DuPont SHIELD Technology with high flow and e.. |