Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 14.1 GPa @Strain 0.680 %, Temperature 23.0 °C |
2050 ksi @Strain 0.680 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 92G45DH2 BK083 Polyphthalamide (PPA) 35% Glass Reinforced PPA High Performance Polyamide with DuPont Zytel HTN92G45DH2 BK083 is a 45% glass reinforced high performance polyamide resin using DuPont SHIELD Technology with high flow and e.. |
|||
Secant Modulus | 14.2 GPa @Strain 1.61 %, Temperature -40.0 °C |
2050 ksi @Strain 1.61 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 545 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 45% Glass Reinforced Polyethylene Terephthalate Rynite 545 NC010 is a 45% glass reinforced modified polyethylene terephthalate with greater strength and stiffness excellent dimensional stability and.. |