Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 1.612 GPa @Strain 5.00 %, Temperature 0.000 °C |
233.8 ksi @Strain 5.00 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500PE BK602 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE BK602 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi.. |