Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 1.94 GPa @Strain 3.30 %, Temperature 40.0 °C |
281 ksi @Strain 3.30 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK641FR NC010 Polybutylene Terephthalate (PBT) 10% Glass Reinforced Flame Retardant Polybutylene Terephthalate Information provided by DuPont Performance Polymers |
|||
Secant Modulus | 1.94 GPa @Strain 0.500 %, Temperature 80.0 °C |
281 ksi @Strain 0.500 %, Temperature 176 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G13L NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Polyamide 66Zytel 70G13L NC010 is a 13% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |