Mechanical Properties Metric English Comments
Secant Modulus 2.05 GPa

@Strain 0.230 %,
Temperature 0.000 °C
298 ksi

@Strain 0.230 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® BM6450XD BK560 Polybutylene Terephthalate (PBT)  (Unverified Data**)&
Unreinforced Polybutylene Terephthalate Developed for Blow MoldingCrastin BM6450XD BK560 is an unreinforced supertough polybutylene terephthalate resin with very high viscosity for extrusion and blo..
Secant Modulus 2.06 GPa

@Strain 2.00926 %,
Temperature 80.0 °C
298 ksi

@Strain 2.00926 %,
Temperature 176 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK612SF NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
15% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK612SF is a 15% glass fiber reinforced low viscosity polybutylene terephthalate for injecti..
Copyright © lookpolymers.com All Rights Reserved