Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 3.03 GPa @Strain 1.50 %, Temperature 40.0 °C |
440 ksi @Strain 1.50 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK601 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 10% Glass Reinforced Polybutylene Terephthalate Crastin SK601 NC010 is a 10% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Secant Modulus | 3.03 GPa @Strain 1.50 %, Temperature 80.0 °C |
439 ksi @Strain 1.50 %, Temperature 176 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK643FR NC010 Polybutylene Terephthalate (PBT) 20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK643FR is a flame retardant 20% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.8.. |
|||
Secant Modulus | 3.03 GPa @Strain 1.10 %, Temperature -40.0 °C |
439 ksi @Strain 1.10 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 520MP NC010 Acetal (POM)
(Unverified Data**) 20% Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 520MP is a medium viscosity acetal homopolymer containing 20% Teflon PTFE Micropowder. It is designe.. |
|||
Secant Modulus | 3.03 GPa @Strain 2.92 %, Temperature 23.0 °C |
440 ksi @Strain 2.92 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 73G30T NC010 Nylon 6
(Unverified Data**) 30% Glass Reinforced Toughened Polyamide 6 Zytel 73G30T NC010 is a 30% glass fiber reinforced toughened polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |