Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 3.29 GPa @Strain 3.50 %, Temperature 40.0 °C |
477 ksi @Strain 3.50 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK605 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Crastin SK605 NC010 is a 30% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Secant Modulus | 3.29 GPa @Strain 1.50 %, Temperature 40.0 °C |
478 ksi @Strain 1.50 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK641FR NC010 Polybutylene Terephthalate (PBT) 10% Glass Reinforced Flame Retardant Polybutylene Terephthalate Information provided by DuPont Performance Polymers |