Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 3.94 GPa @Strain 0.250 %, Temperature 100 °C |
571 ksi @Strain 0.250 %, Temperature 212 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK643FR NC010 Polybutylene Terephthalate (PBT) 20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK643FR is a flame retardant 20% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.8.. |
|||
Secant Modulus | 3.94 GPa @Strain 0.900 %, Temperature -40.0 °C |
572 ksi @Strain 0.900 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 900P BK602 Acetal (POM)