Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 2.3388 GPa @Strain 5.67 %, Temperature -40.0 °C |
339.22 ksi @Strain 5.67 %, Temperature -40.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 132F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 132F NC010 is a nucleated lubricated polyamide 66 for injection molding. It was developed for fast production cycles and high productivity applications.Info.. |