Mechanical Properties Metric English Comments
Secant Modulus 2.5695 GPa

@Strain 2.00 %,
Temperature -20.0 °C
372.68 ksi

@Strain 2.00 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® 6130 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin 6130 NC010 is an unreinforced medium high viscosity polybutylene terephthalate resin for ..